Sign In | Join Free | My burrillandco.com |
|
Ask Lasest Price | |
Brand Name : | LFPCO |
Certification : | ISO9001:2015 |
Additional Requirement for DSS Material from COMPANY
Charpy V-Notch (ASTM A370)
Not applicable when the maximum obtainable Charpy specimen width
less than 2.5mm Absorbed energy shall be 61J average and 48J Single
value minimum Test temperature shall be minus 46 deg C. Impact test
specimen taken from mid-thickness position.
Ferrite Count (ASTM ES62)
Ferrite content shall be determined by manual point count on a
cross section near OD, ID surface & midwall location. Sample shall
be electrolytically etched in NaOH or KOH, and in such a manner as
to provide optimum contrast for austenite and ferrite phase
discrimination. Minimum 30 field and 16 points per field shall be
used. Ferrite content shall be between 40% to 60%.
Metallographic Examination
Sample shall be etched using ASTM E407, K3Fe (CN)6 with KOH or
NaOH. Sample cross section shall be examined at OD, ID and midwall
locations. Examination shall be conducted at a minimum of 400X to
500X magnification. Material shall be free of intermetallic phases
and precipitates A microphotograph at a minimum of 400X to 500X
shall be supplied.
Corrosion Test
Shall be carried out as per ASTM G4S at 25 deg C for 24 hours with
an acceptance criteria of no visual pitting at 20X and weight loss
of less than 4 g/m2.
NACE Hardness
Hardness test according to NACE MR-0175 the maximum shall be HRC
28, HB 271, or HV10 310.
Other Requirements
CONTRACTOR/COMPANY representative examination required for heat
number traceability, visual examination, dimensional examination
and mill test certificate review. All testing required to be per
heat number.
NOTE:
Duplex Stainless Steel (DSS)
All DSS Material shall be in accordance with a minimum PREN of 34
according to the formula:
PREN = %Cr + 3.3×(%Mo + 0.5×%W ) + 16×%N
![]() |